Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Is it possible to have a modulus of elasticity 800ksi using E/R glass?

Status
Not open for further replies.

jgpower

Structural
Joined
Nov 8, 2006
Messages
8
Location
US
Hi everyone,

Is it possible to achieve a modulus of elasticity 800 ksi using common glass fibers such as E glass, R glass or S glass, not carbon fibers? I am looking for a composite I profile instead of aluminu I profile within some limits on dimensions of the I section. I need a high modulus because of deflection limit.

Any reply is appreciated.

11/08/06
 
Glass/epoxy unidirectional tape as a modulus ~6 msi; glass/epoxy fabric has a modulus ~ 3 msi.
 