My answer is no, don't get zinc in contact with stainless steel. Despite of some contrary opinions, I still call two reasons for it;- the localised preferential galvanic corrosion will remove the zinc coating, exposing the B7 bolts to the marine environment and also, in case of hign temperature exposure, the chemical reaction between the zinc and the stainless could be an additional fire hazard. That's valid for the coated washers also.
cheers,
gr2vessels