The design code is B 31.3. Production uses heat extensively to align the joints and we are talking about 304H steel small size piping (pig tails). It's GTAW welding, so they simply use the rod tip to heat the existing weld and sometimes the joint comes into position without additional force applied, just due to thermal shrinkage but sometimes they also apply some force. Is this a point of concern?