Is the material duplex 2507 considered the same material as Inco 825?u
 
Replies continue below

Recommended for you

No.

2507 is a dual phase austenitic-ferritic duplex stainless steel. Inconel 825 is an austenitic nickel based alloy. They have different mechanical properties and corrosion performance.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 