Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Is CRCA steel good enough for Outdoor electronics applications?

Status
Not open for further replies.

schwarz

Electrical
Joined
Jan 14, 2002
Messages
29
Location
IN
Hi, Normally we use aluminum cabinets for outdoor electronics enclosure. To reduce cost we propose use of CRCA steel. Please suggest if this is OK and what type of plating and painting are required to achieve 10yr+ life.Regards
 
You could use an automotive like finish--start with E-Coat, then primer, then top coat. You could also do powder coat over the E-coat, as long as your coater understands how to get good coverage in the corners.
 
Thanks swall, what would be plating/galvanising recommendation? [ I am not from this background]
 
Two options:

galvanized steel (~ 40 micrometers thickness) + paint (your choice, urethanes are good topcoats since they are UV resistant)

bare steel + zinc phosphate (a primer) + epoxy-based cathodic electrocoat (~ 30 micrometers thick) + topcoat (urethane-based is a good choice).
 