Hi,
A carbon steel pressure vessel to be manufactured per
ASME Section IX requirements needs overlay of Cu/Ni 70/30.
The vessel case is manufactured and then the overlay
is applied. The overlay layer is not stressed by manufacturing procedures, beyond welding shrinkage stresses. It is stress relieved after overlay.
Test specimens with overlay fail upon bending.
Is bend testing for welded overlay really required per ASME Sect. IX?
Thanks.
A carbon steel pressure vessel to be manufactured per
ASME Section IX requirements needs overlay of Cu/Ni 70/30.
The vessel case is manufactured and then the overlay
is applied. The overlay layer is not stressed by manufacturing procedures, beyond welding shrinkage stresses. It is stress relieved after overlay.
Test specimens with overlay fail upon bending.
Is bend testing for welded overlay really required per ASME Sect. IX?
Thanks.