Is ASTM A 234 WP12 Equal To AISI 4140 1

Status
Not open for further replies.

mmbguide

Mechanical
Joined
Apr 8, 2016
Messages
38
Location
DE
hello

Is "ASTM A 234 WP12" equal To "AISI 4140"?

thank you
 
No, it is not.

Chemically with Chromium and Molybdenum, they are close, but the big difference between the two is the amount of Carbon.

WP12: C = 0.05-0.20%
4140: C = 0.38-0.43%



The devil is in the details; she also wears prada.
 