Dec 30, 2010 #1 wagnermj Chemical Joined Mar 17, 2010 Messages 15 Location US I was wondering if A-108 grade 1018 (round bar P-1 group 1)is a recognized material by ASME (SA designation). I plan to machine bar stock to make plugs for a repair to a heat exchanger, and the MTR that I received only shows an ASTM designation.
I was wondering if A-108 grade 1018 (round bar P-1 group 1)is a recognized material by ASME (SA designation). I plan to machine bar stock to make plugs for a repair to a heat exchanger, and the MTR that I received only shows an ASTM designation.
Dec 30, 2010 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US No, this is not an ASME material speecification. Upvote 0 Downvote
Dec 30, 2010 Thread starter #3 wagnermj Chemical Joined Mar 17, 2010 Messages 15 Location US Is there an ASME equivelent to A-108-1018 Upvote 0 Downvote
Dec 30, 2010 #4 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Try SA 105. Upvote 0 Downvote
Dec 30, 2010 #5 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Also try SA 696 Grade B. Upvote 0 Downvote