Oct 15, 2002 #1 majordud Industrial Joined Mar 9, 2002 Messages 8 Location US Does anyone have, or know where I can get a good digital copy of the Iron-Carbon diagram?
Oct 15, 2002 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US I went to http://www.google.com, clicked on Images and typed "Iron-carbon phase diagram". The results can be obtained by clicking on the following link: http://images.google.com/images?q=Iron-carbon+phase+diagram&ie=ISO-8859-1&hl=en Upvote 0 Downvote
I went to http://www.google.com, clicked on Images and typed "Iron-carbon phase diagram". The results can be obtained by clicking on the following link: http://images.google.com/images?q=Iron-carbon+phase+diagram&ie=ISO-8859-1&hl=en
Oct 15, 2002 #3 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US ASM International has one in its Metals Handbook Desk Edition, which is available to members on the web for free. The cost of membership is only $100. Learn more at: http://www.asminternational.org Upvote 0 Downvote
ASM International has one in its Metals Handbook Desk Edition, which is available to members on the web for free. The cost of membership is only $100. Learn more at: http://www.asminternational.org
Oct 15, 2002 #4 Rich2001 Mechanical Joined Mar 23, 2001 Messages 896 Location US Tempil has a nice diagram. A copy can be found at http://www.abana.org/resources/education/tempil_guide.html Upvote 0 Downvote
Tempil has a nice diagram. A copy can be found at http://www.abana.org/resources/education/tempil_guide.html
Oct 15, 2002 #5 AlanD Materials Joined Apr 2, 2001 Messages 63 Location AU Also available here with a large number of other phase diagrams. http://cyberbuzz.gatech.edu/asm_tms/phase_diagrams/#periodic_table Upvote 0 Downvote
Also available here with a large number of other phase diagrams. http://cyberbuzz.gatech.edu/asm_tms/phase_diagrams/#periodic_table
Oct 15, 2002 Thread starter #6 majordud Industrial Joined Mar 9, 2002 Messages 8 Location US Thanks guys/gals/whatevers. Found what I was looking for. You were all a big help. End this thread. Upvote 0 Downvote