We are having a problem with wear on a 1/8' thk 4130 sheet metal lever. Currently the lever is Q&T to 50 HRC.
We are thinking about taking the existing levers and having them Ion Nitrided about 0.010" deep and then possibly PVD coating.
I am aware that the 50 HRC lever would decrease in hardness to about 35 HRC but this would be acceptable as long as the nitrided case was in the 55 HRC or greater range.
Am I going in the right direction here? Could someone recommend a PVD coating that could be applied over the nitriding?
We are thinking about taking the existing levers and having them Ion Nitrided about 0.010" deep and then possibly PVD coating.
I am aware that the 50 HRC lever would decrease in hardness to about 35 HRC but this would be acceptable as long as the nitrided case was in the 55 HRC or greater range.
Am I going in the right direction here? Could someone recommend a PVD coating that could be applied over the nitriding?