Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Investment casting of Al 356

Status
Not open for further replies.

triumph406

Aerospace
Joined
Oct 28, 2005
Messages
47
Location
US
Hi,
I am contemplating casting a product in Al 356. If I make a mold to make wax patterns, does anybody know the allowance I need to apply to apply to the cavity to account for the wax shrinkage, and the Al shrinkage.
Regards Dave
 
Hi,

approximate shrinkage allowance for wax 0.4%

approximate shrinkage allowance for Al alloys 1.1 - 1.3 %

approx. total allowance 1.5 - 1.7 %

Hoping this helps, with regards,


 
Thanks for the details, I will try some sample parts and use your values as a starting point. I'm trying to match an existing part so I want to able to match the size closely, so it may take some trial and error.
Thanks
 