Aug 17, 2006 #1 becma27 Mechanical Joined May 20, 2002 Messages 21 Location US Hi all, I'm looking to plate a piece of Invar 36 with a low reflectivity black surface similar to a black anodize for aluminum. Also needs to be a low-outgassing apporoach. Any suggestions and/or specifications to call out? Thx.