Does anybody have any experience of casting and/or machining Invar 36?

What are the pitfalls to watch for, and are there any little tricks I should know.

Many thanks.
 
Replies continue below

Recommended for you

bruv,I have made castings in invar 36 and there are a whole lot of issues in getting a sound casting. If you could let me know the part to be cast and the process is being adopted for manufacture,I can share some of my experiences.
 