A supplier has proposed a fabric that meets MIL C 20696 which requires testing after Accelerated Weathering per FED 191. My customer wants to know the "approximate life expectancy" of the fabric outdoors. The testing / MIL spec doesnt put the results in terms of life expectancy. Is there a way to equate the 150 hours of Accelerated weathering to actual outdoor exposure?