Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Interpretation UW-13.3 Sketch (c) for Tube sheet with Hub 1

Status
Not open for further replies.

Safwan Chaklasiya

Mechanical
Joined
Oct 28, 2022
Messages
1
Location
IN
thread292-471709

Question

In design of Heat exchanger with hub type Tube sheet as per Fig UW-13.3 sketch (c). Tube-sheet thickness is 150 mm and adjacent shell thickness is 68 mm.
My question is " Is corner radius requirement as per Note(a) - figure UG-34 sketch (b-2), is applicable for sketch(C) of figure UW-13.3. "

My understanding :
-As radius requirement is not explicitly mentioned in sketch (C) of below figure the way it is mentioned for sketch (a) & (b), radius as per sketch (b-2) of fig UG-34 is not applicable.
-In my job, shell thickness is 68 mm and we have provided corner radius of 10 mm.
If UG-34 is applicable then corner radius comes to 19 mm. With 19 mm corner radius tube holes falls on radius profile, which further create problem in tube # tube-sheet welding

Answer

As per ASME Interpretation 20-260 (refer below link), radius need not to be followed as per sketch (b-2) of fig UG-34 for sketch(c) of figure UW-13.3.

 
Safwan Chaklasiya, good to know. Thx :)

EDIT: would have been nice had the interp confirmed / denied the minimum radius.