Hi,
I am designing Heat exchanger with hub type Tube sheet as per Fig UW-13.3 sketch (c). Tube-sheet thickness is 150 mm ans adjacent shell thickness is 68 mm.
My question is " Is corner radius requirement as per Note(a) - figure UG-34 sketch (b-2), is applicable for sketch(C) of figure UW-13.3. "
My understanding :
-As radius requirement is not explicitly mentioned in sketch (C) of below figure the way it is mentioned for sketch (a) & (b), radius as per sketch (b-2) of fig UG-34 is not applicable.
-In my job, shell thickness is 68 mm and we have provided corner radius of 10 mm.
If UG-34 is applicable then corner radius comes to 19 mm. With 19 mm corner radius tube holes falls on radius profile, which further create problem in tube # tube-sheet welding
Please suggest.
Regards
Nikunj
I am designing Heat exchanger with hub type Tube sheet as per Fig UW-13.3 sketch (c). Tube-sheet thickness is 150 mm ans adjacent shell thickness is 68 mm.
My question is " Is corner radius requirement as per Note(a) - figure UG-34 sketch (b-2), is applicable for sketch(C) of figure UW-13.3. "
My understanding :
-As radius requirement is not explicitly mentioned in sketch (C) of below figure the way it is mentioned for sketch (a) & (b), radius as per sketch (b-2) of fig UG-34 is not applicable.
-In my job, shell thickness is 68 mm and we have provided corner radius of 10 mm.
If UG-34 is applicable then corner radius comes to 19 mm. With 19 mm corner radius tube holes falls on radius profile, which further create problem in tube # tube-sheet welding
Please suggest.