In the manufacturing of a reducer per ASTM A403 Gr.WP 321 Cl. WX (100%RT).
A manufacturer welded with control of maximum interpass temperature at 200 Deg.C. In my welding knowledge, this is too high for maximum interpass temperature and crack resistibility deteriorates with high interpass temperature.
Please comment for this case...Is this high interpass temperature for welding austenitic stainless steel accepted by other customers?