May 21, 2012 #1 Makun Mechanical Joined Jul 20, 2009 Messages 57 Location AR Hi! Which is the best practice for inspection pressure vessels with internal lining? Do you have any recommended bibliography?
Hi! Which is the best practice for inspection pressure vessels with internal lining? Do you have any recommended bibliography?
May 21, 2012 #2 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US If paint type lining, holiday testing, dry film thickness testing and visual testing as a minimum should be required for finished coating. You need to define type of coating; i.e., paint type, elastomeric, alloy clad, weld overlay, etc. Upvote 0 Downvote
If paint type lining, holiday testing, dry film thickness testing and visual testing as a minimum should be required for finished coating. You need to define type of coating; i.e., paint type, elastomeric, alloy clad, weld overlay, etc.
May 21, 2012 Thread starter #3 Makun Mechanical Joined Jul 20, 2009 Messages 57 Location AR Is there some efective method to be applied in service? Upvote 0 Downvote
May 25, 2012 #4 rustbuster Petroleum Joined Jul 7, 1999 Messages 289 Many, what type of lining and what are you looking to find with your inspection? Upvote 0 Downvote
May 28, 2012 Thread starter #5 Makun Mechanical Joined Jul 20, 2009 Messages 57 Location AR The kind of Coating is Epoxy , I want to verify the integrity of the coating and find corrosion zones Upvote 0 Downvote
The kind of Coating is Epoxy , I want to verify the integrity of the coating and find corrosion zones
May 28, 2012 1 #6 rustbuster Petroleum Joined Jul 7, 1999 Messages 289 This would require internal inspection and Holiday testing. Upvote 0 Downvote