I'm soon going to be observing the installation of auger cast piles for the first time.
Any tips on things to look for when observing?
Any tips on things to look for when observing?
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
Count the pump strokes. Know the volume of each stroke.
Make sure there is sufficient head on the grout to prevent "necking" of the pile.
Compare pumped volume with theoretical pile volume. If different, find out why. If actual < theoretical....necking. If actual > theoretical, low strength stata or lense encountered, or void in soil profile.