We are welding a 1 1/4" thick pile on site with a SIngle Bevel Groove Joint with a backing Ring. The weld is in 2G position. There is no access to get in once the welding is done. We are trying to figure out the kind of Inspection testing to be done on the weld. Is there any specifications for this weld? If so can I please have the Code name?

Thank You
Keshav Vasudevan
 
I would suggest ultrasonic flaw detection, using either criteria of the American Welding Society (AWS), D1.1-Structural Welding Code-Steel, or similar (ANSI B31.1).
 