Good morning,
We have a production Separator (3 phases, Design Pressure 7 bar, Design Temperature 90 Degrees Celsius) that will undergo general 5-year inspection.
During this scheduled inspection program, is it necessary to completely strip a separator from its insulation to check the exterior surfaces condition?
Is it also necessary to remove the insulation around the nozzles to inspect their external welding to the shell or it is enough to check internally?
If the situation inside the separator is good, does it required to grind the painting of the nozzles' welding to perform MPI Magnetic Particles Inspection on them?
Finally, which are the standard API 510 requirements for the planned internal & external inspections for Pressure Vessels?
Thanks and best regards,
We have a production Separator (3 phases, Design Pressure 7 bar, Design Temperature 90 Degrees Celsius) that will undergo general 5-year inspection.
During this scheduled inspection program, is it necessary to completely strip a separator from its insulation to check the exterior surfaces condition?
Is it also necessary to remove the insulation around the nozzles to inspect their external welding to the shell or it is enough to check internally?
If the situation inside the separator is good, does it required to grind the painting of the nozzles' welding to perform MPI Magnetic Particles Inspection on them?
Finally, which are the standard API 510 requirements for the planned internal & external inspections for Pressure Vessels?
Thanks and best regards,