RE: inspection of CJP at moment connection vs prequalified joint
connectegr, I need some of that CWI support for a field welding/bolting issue...question: On a CJP beam to column moment connection, the prequalified joint designation shown is TC-U4a, but have a situation where the column appears to have cut a little short resulting in the bottom of the top beam flange being actually equal to the top of column cap plate. Not exactly the prequalified joint...
What should be the proposed fix on this?
connectegr, I need some of that CWI support for a field welding/bolting issue...question: On a CJP beam to column moment connection, the prequalified joint designation shown is TC-U4a, but have a situation where the column appears to have cut a little short resulting in the bottom of the top beam flange being actually equal to the top of column cap plate. Not exactly the prequalified joint...