Feb 13, 2013 #1 Tman1 Petroleum Joined Dec 5, 2012 Messages 25 Location ZA insp-123 Hy all just wanna know which one is better material grade in ss 316-L/304-L....can i use 316-L instead of 304-L or vice versa.
insp-123 Hy all just wanna know which one is better material grade in ss 316-L/304-L....can i use 316-L instead of 304-L or vice versa.
Feb 13, 2013 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Not enough information to provide an answer. What is the expected service conditions for the above - temperature, environment, etc. Upvote 0 Downvote
Not enough information to provide an answer. What is the expected service conditions for the above - temperature, environment, etc.
Feb 13, 2013 #3 EdStainless Materials Joined May 20, 2004 Messages 16,399 Location Waukesha WI USA Mechanically they are very similar, so if there is no corrosion go ahead. Otherwise we need to know specifics about the environment. = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote
Mechanically they are very similar, so if there is no corrosion go ahead. Otherwise we need to know specifics about the environment. = = = = = = = = = = = = = = = = = = = = Plymouth Tube
Feb 13, 2013 #4 metman Materials Joined Feb 18, 2002 Messages 1,187 Location US If the ss is to be welded, 316L is more forgiving than 304L for sensitization. But as metengr says more info needed. Design for RELIABILITY, manufacturability, and maintainability Upvote 0 Downvote
If the ss is to be welded, 316L is more forgiving than 304L for sensitization. But as metengr says more info needed. Design for RELIABILITY, manufacturability, and maintainability
Feb 13, 2013 Thread starter #5 Tman1 Petroleum Joined Dec 5, 2012 Messages 25 Location ZA Its a reformed gas-commodity operating at 2340 kpa and 157 degrees celcius....4 inch Upvote 0 Downvote