Sep 10, 2010 #1 Koros Mechanical Joined Aug 31, 2010 Messages 18 Location NL For welding a shell of stack with 3300 mm I.D. and thickness range 15 to 8 mm, inside or outside groove on circumferential and longitudinal seams of stack is preferable.
For welding a shell of stack with 3300 mm I.D. and thickness range 15 to 8 mm, inside or outside groove on circumferential and longitudinal seams of stack is preferable.
Sep 10, 2010 #2 CorBlimeyLimey Mechanical Joined Nov 5, 2003 Messages 15,292 Location CA You may have better responses in forum725 ... and a little more info would be helpful. Does the "shell" keep stuff in or out? What stuff? What environment? What material? Upvote 0 Downvote
You may have better responses in forum725 ... and a little more info would be helpful. Does the "shell" keep stuff in or out? What stuff? What environment? What material?