I am working on an existing steel framed building (design drawings dated 1962) where two different deck systems are listed on the drawings as"
"Inland Deck BB 16-16" - Multiple span with beams at 10'-0" on center. Per details, the deck is 3" with either 2" or 2-1/2" concrete
"Inland Deck BC 12-12" - Single span of 20'. Per details, the deck is 6" with 2" or 2-1/2" concrete.
I have been unable to locate any information on the Inland deck. Does anyone have any contacts/old manuals they would be willing to share or anything else that would be helpful in assisting in verifying the existing system from a capacity and weight standpoint?
thanks
pat
"Inland Deck BB 16-16" - Multiple span with beams at 10'-0" on center. Per details, the deck is 3" with either 2" or 2-1/2" concrete
"Inland Deck BC 12-12" - Single span of 20'. Per details, the deck is 6" with 2" or 2-1/2" concrete.
I have been unable to locate any information on the Inland deck. Does anyone have any contacts/old manuals they would be willing to share or anything else that would be helpful in assisting in verifying the existing system from a capacity and weight standpoint?
thanks
pat