Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Injector lances for big diameter, feeder for RO process

Status
Not open for further replies.

Carreroal

Mechanical
Jan 27, 2020
6
Hi everyone, I working in a injection chemical process for entrance of RO system, and the principal Pipe of feed system have 2600 mm of diameter. We have a proposal for material. We think in teflon for all the body of this injector with 30ª of inclination respect to the vetical.

Any of you have experience about materials and injectors for big diamenters? (1.8 m/s fluid velocity)