Hello the ultimate engineering forum, now that i have changed my focus from metallugry to fea - i need your help with rubber bushings in Ansys Workbench 13. I can get the solution to converge fine even with frictional contacts - no issues. However, i dont know where to start on the real distorted bushings and oval bar from bending.
Working solution: use perfect round shaft and round bushing, do not account for any bracket preload that will compress parts of the bushing prior to loading (during vehicle installation). - that works great.
Non working solution: how do i put a round bushing around an oval bar and obtain the proper compression in the rubber as the bracket tightens around the rubber busihng that is trying to conform to the oval steel bar? That is what i need for the initial condtion, and then i can apply the loads. the perfect round and even bushing pressure scenario above isn't real.
is there a bible or anything i can read on how to obtain this pre-loaded rubber. ps, NO I have not got non-linear large displacement to converge yet using actual rubber hyper elastic curves so for now i'm just practicing using a simple linear elastic material with a high poissons ratio and weak E. (looks cool flexing all around, freakin real hyper elasic is the next level up in difficulty.)
thanks for reading, hope i can help others here too.
Working solution: use perfect round shaft and round bushing, do not account for any bracket preload that will compress parts of the bushing prior to loading (during vehicle installation). - that works great.
Non working solution: how do i put a round bushing around an oval bar and obtain the proper compression in the rubber as the bracket tightens around the rubber busihng that is trying to conform to the oval steel bar? That is what i need for the initial condtion, and then i can apply the loads. the perfect round and even bushing pressure scenario above isn't real.
is there a bible or anything i can read on how to obtain this pre-loaded rubber. ps, NO I have not got non-linear large displacement to converge yet using actual rubber hyper elastic curves so for now i'm just practicing using a simple linear elastic material with a high poissons ratio and weak E. (looks cool flexing all around, freakin real hyper elasic is the next level up in difficulty.)
thanks for reading, hope i can help others here too.