Guys:
We have several pipelines varying in length and diameter, up to 35kms in length and dia of 10" - 24" that are going to be hydrotested and left full of water until commissioning - they may lay in "storage" for a year+.
Nitrogen is not an option, and de-watering, drying and leaving it full of "dry" air has been ruled out.
The pipelines will be laid offshore in shallow water (18m maximum).
As far as an inhibitor mix, what has been proposed (by Nalco) is the following:
1 - EC1304A, a water soluble, oil dipersible corrosion inhibitor effecitvie in fresh & brine water & offers protection from H2s and CO2 corrosion - 100PPM
2 - EC6064A, an ammonium bisulfate oxygen scavenger used to prevent oxygen corrosion - 60PPM
3 - EC6197A, a water soluble aldehyde with quaternary ammonium compound for control of aerobic and anaerobic bacteris - 250PPM
Does anyone see any issues with the proposed inhibitor mix?
Greg Lamberson, BS, MBA
Consultant - Upstream Energy
Website:
We have several pipelines varying in length and diameter, up to 35kms in length and dia of 10" - 24" that are going to be hydrotested and left full of water until commissioning - they may lay in "storage" for a year+.
Nitrogen is not an option, and de-watering, drying and leaving it full of "dry" air has been ruled out.
The pipelines will be laid offshore in shallow water (18m maximum).
As far as an inhibitor mix, what has been proposed (by Nalco) is the following:
1 - EC1304A, a water soluble, oil dipersible corrosion inhibitor effecitvie in fresh & brine water & offers protection from H2s and CO2 corrosion - 100PPM
2 - EC6064A, an ammonium bisulfate oxygen scavenger used to prevent oxygen corrosion - 60PPM
3 - EC6197A, a water soluble aldehyde with quaternary ammonium compound for control of aerobic and anaerobic bacteris - 250PPM
Does anyone see any issues with the proposed inhibitor mix?