Hi dear colleagues
what are ways for protection of stainless steel cladding against chloride ion saturated water?
 
Replies continue below

Recommended for you

Alloy with Mo at a concentration near 6 % by mass.
 
Not by chemically treating the water, only by using a better alloy.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
We could hope you mean "insulation cladding", in which case the answer would be "paint"...

If you mean "internal vessel cladding", you're beat-
 
Well, raising the sulfate level will lessen the impact of the chlorides slightly. This isn't a practical inhibition method.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
hi dear colleagues and thanks for your attentions
I mean "internal vessel cladding" and the water cut of petrolume flude has 10000 ppm chloride salts and temperature is between 60 and 100 C degree. we inject a water soluble inhibitor but the Fe content in outlet water from seperator is high.
 