I am looking for an Infrared sensor for measuring TIG welding temperature at every pass (interpass temperature). Should I go for a fixed or variable emissivity instrument?

What is the difference between the two realy?

Thanks!
 
Replies continue below

Recommended for you

Here is a website that could be helpful.
Here is another good website
Another good link
Heckler [americanflag]
Sr. Mechanical Engineer
SWx 2007 SP 4.0 & Pro/E 2001
o
_`\(,_
(_)/ (_)

This post contains no political overtones or undertones for that matter and in no way represents the poster's political agenda.
 
I would go for the variable emissivity since I assume you want to measure the molten metal? And I also assume there will be some sort of protective shield? By using a variable sensor you can calibrate for your specific set-up. ISZ
 