The contractor poured a portion of a slab on ground 2-1/2" too low. He thought it was a depressed slab, but it is not. The existing slab is 6 inches thick with 4x4 W4.0xW4.0 WWF. The rooms are mostly for storage and will have vinyl composition tile.
The contractor’s solution is to apply a bonding agent and infill the 2 -1/2” with a 4,000 psi grout. I have asked that he submit a mix design along with break data.
This seems acceptable to me, what do you think?
The contractor’s solution is to apply a bonding agent and infill the 2 -1/2” with a 4,000 psi grout. I have asked that he submit a mix design along with break data.
This seems acceptable to me, what do you think?