Oct 26, 2020 #1 Vxxxxx Mechanical Joined Jun 5, 2020 Messages 91 Location MY Hi, I wonder how to obtain the value of inelastic heat fraction for a certain material. The default value is 0.9. Thank you.
Hi, I wonder how to obtain the value of inelastic heat fraction for a certain material. The default value is 0.9. Thank you.
Oct 26, 2020 #2 FEA way Mechanical Joined Nov 13, 2018 Messages 5,193 Location PL You would have to carry out some physical experiments or use value from literature. Otherwise you can leave the default value. Upvote 0 Downvote
You would have to carry out some physical experiments or use value from literature. Otherwise you can leave the default value.
Oct 26, 2020 Thread starter #3 Vxxxxx Mechanical Joined Jun 5, 2020 Messages 91 Location MY Okay thank you very much, FEA way. Upvote 0 Downvote