jvazquez87
Electrical
Im learning about induction furnaces and recently came across this site. I love it! i hope i can ask for help on things i can't quite find out on my own. So my first issue is im wanting to build a furnace for the purpose of casting steel in specific I'm wanting to be able to cast tool steel for use in the production of quality anvils and various other tools. I want to keep it small with a target casting ability of up to 200lbs in a single cast. So i have a few questions for the knowledgeable people here.
1.I know that induction furnaces use high quality copper tubing for the coils like here Link I'm trying to figure out how big of a furnace i will need to build to be able to cast up 200lbs of steel and also what size coils i would be ok to use. What are the acceptable wall thickness of copper for this type of application? What kind of volts/current would i need to power such a furnace? Any help is greatly appreciated.
2.Also for this amount of steel would i be able to use another source of heat such as a waste oil burner? mix with propane? i was thinking about using propane or oil and pressurizing it with pure oxygen instead of high pressure air... These are just ideas i thought about floating around and seeing if someone could help. Thank you for your time.
3.Finally for today i have a plant in my town that produces refractory material but they only produce it for the aluminum industry, from what I've learned they carry a high alumina mix for certain alloys that theoretically would be suitable for use in steel. Im wanting to stay with a crucible type of pour for the sake of ease and plan to build the tools that are needed as i dont think 200lbs would be too much for 2 people to handle. I'm definitely thinking about safety first and plan to make it as remote a process as i can realistically.
Ill see if i can draw up some ideas and get some input from you guys. Thanks hope to hear back soon.
1.I know that induction furnaces use high quality copper tubing for the coils like here Link I'm trying to figure out how big of a furnace i will need to build to be able to cast up 200lbs of steel and also what size coils i would be ok to use. What are the acceptable wall thickness of copper for this type of application? What kind of volts/current would i need to power such a furnace? Any help is greatly appreciated.
2.Also for this amount of steel would i be able to use another source of heat such as a waste oil burner? mix with propane? i was thinking about using propane or oil and pressurizing it with pure oxygen instead of high pressure air... These are just ideas i thought about floating around and seeing if someone could help. Thank you for your time.
3.Finally for today i have a plant in my town that produces refractory material but they only produce it for the aluminum industry, from what I've learned they carry a high alumina mix for certain alloys that theoretically would be suitable for use in steel. Im wanting to stay with a crucible type of pour for the sake of ease and plan to build the tools that are needed as i dont think 200lbs would be too much for 2 people to handle. I'm definitely thinking about safety first and plan to make it as remote a process as i can realistically.
Ill see if i can draw up some ideas and get some input from you guys. Thanks hope to hear back soon.