Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Indian Boiler regulation

Status
Not open for further replies.

consideritsolved

Mechanical
Feb 9, 2007
16
Can anyone help me understand what this Indian Boiler regulatio (IBR) does? How do we get approval for control valves for IBR?
 
Replies continue below

Recommended for you

If you are a HSBCT customer, visit the web site.
 
My experience of IBR regulations is strictly in refinery pipework.

IBR regulations apply to all steam and associated lines such as boiler feedwater in India. There are specific requirements for materials, wall thickness etc, similar to other design codes.

Results must be produced in a specific form .... stress isometrics showing all restriants, springs etc. This can be very demanding, usually being produced towards the end of a project, and rejection can prevent plant operation.

Good advice ... Treat IBR and its representatives with great respect !!
 
The design and fabrication of boilers has be done in accordance with IS:2825 and other Indian Standards. IBR basically certifies that the boiler conforms to those codes.