I've been asked to confirm a design for a road job in southern India. The design is for 1 million axles for a 15 year period. Specification is for 200mm sub-base, then 250mm hydraulically bound material, topped with 60mm base hma and 40mm wearing course hma. The sub-base cbr is 8. Is this spec over the top or can someone come up with a non asphaltic alternative?
 
Is the 250mm hydraulically bound material identified as WMM or WBM? Will the subbase be crushed stone or river gravel? Lorries in India are notoriously and severly overloaded - your 1 million standard axles may end up effectively to be much much higher.

For a road of which I am aware - a National Highway - and upwards to well over a hundred million axle loads on the life span, 330 crushed stone subbase, 200mm crushed stone base and 210 total bituminous thickness (170 dense base macadam) and 40 wearing course (BC) - on a CBR requirement (light tamping - standard Proctor) of 6 for the underlying 500mm subgrade.

A few things to consider - the mix designs typically now use 4 to 6 percent air voids - used to be 3 to 5% - but the compaction level required by the agency is 98% Marshall - about 2% higher than normal compaction for highways. Contractors always wanted to exceed (and many times more than 100%) because if below 98%, they lost a portion of their bid rate. If below 95% they lost it all in some cases. Secondly, it is very hot and humid - flushing is a big big problem - try to use a polymer modified bitumen - rubber modified can also work - or specify a 30-40 penetration grade. 60-70 has a softening point in the order of 46 to 47 degrees and with April/May temps approaching 46 to 48 with humidity, well, . . . They have not gone to performance grade which would require viscosity decrease for the penetration grades. Top down cracking is also understood to be a problem that should be addressed although many don't yet recognize the mechanism at present.

Just some thoughts - and goooooooooddd luck.
 