tincan
Civil/Environmental
- Aug 8, 2003
- 164
I have an open channel between 2 fixed elevation RCB's. To connect these two I can use a drop structure or a slope of 1.33% which produces high velocities. Has anyone roughened the interior of an RCB, sandblast or water pressure on setting concrete to obtain a higner "n" value?
Would have to go from the normal value of 0.013-0.014 to 0.025 to reduce the velocities to a workable limit.
i would prefer not construction dragon teeth or blocks within the RCB because of possible trash hangup, maintenance is poor.
Anybody tried this?
Would have to go from the normal value of 0.013-0.014 to 0.025 to reduce the velocities to a workable limit.
i would prefer not construction dragon teeth or blocks within the RCB because of possible trash hangup, maintenance is poor.
Anybody tried this?