vcz
Mechanical
- Aug 23, 2002
- 6
Hello,
I am having trouble with a heavy clutch plate with internal
spline teeth. The part is 16"OD 5"ID 1.1"thick 8620 steel.
After case-hardening 54-58Rc .040"total deep, the pitch dia.
of the spline grows .020"-.040" on different parts in the same heat. Is this to be expected?
I am having trouble with a heavy clutch plate with internal
spline teeth. The part is 16"OD 5"ID 1.1"thick 8620 steel.
After case-hardening 54-58Rc .040"total deep, the pitch dia.
of the spline grows .020"-.040" on different parts in the same heat. Is this to be expected?