I need Rockwell Hardness data for Inconel 718 in the following forms [or equivalent]:

Inconel 718 per AMS5662: Solution HT
Inconel 718 per AMS5663: Solution HT & Precipitation HT

NOTE: I need MIN and MAX hardness values for range comparison.

NOTE: If You know the MIN and MAX corresponding FTy [relative to hardness] I would also appreciate this info. Regards, Wil Taylor
 
Replies continue below

Recommended for you

Hush & TVP...

The Special Metals website You both listed has the exact Info I was looking for... and much more!

Regards, Wil Taylor
 