Does anyone know where I can obtain fracture toughness data for Inconel 718 down to -423 F for the two different applied heat treatments AMS 2774 S1950DP and S1750SDP?
I would try to look at the CINDAS data developed via Wright Patterson AFB. This came in book form and may still be available as such, but it is also in a database. The data is the most comprehensive I've seen for a given alloy. Their link is