Hi,

I have some large forgings I need manufactured in Inconel 718 (approximately DIA1000mm x 200mm with a bore of 700mm). Can anybody recommend a supplier that may be able to supply these. We are based in the UK but anticipate having to use a US supplier or somewhere in the Far East.

Thanks
 
Replies continue below

Recommended for you

Repost this issue to Metals/Metallurgy forum...
SPECIFICALLY state [at minimum] alloy/procurement specification, heat-treat condition/specification and size [+ max X-section/depth] of the proposed forging.

Regards, Wil Taylor
o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 