What is the difference between incoloy 800H and 800 AT ?
What are the areas of appication ?
What are the merits of 800 H over 800 AT ?
 
My suggestion is to visit the comprehensive web site below by Special Metals for excellent technical background on Incoloy materials. They can answer all of your questions.

 
Thanks metengr. However this site has no information about incoloy-800AT
 
I have one reference that refers to AMS 5871 which is the same for Incoloy 800.
 
Chemically they are the same. the difference is in the heat treating. H or HT is heat treated for higher strength, AT is annealed.
 
Be aware that if you use Inc.800 types and the sum of Ti+Al is more than 0,7%, PWHT is nescessary when the operation temperature is between 500 - 750 C.
Reason : prevention stress induced cracking during operation. A crack type that occurs within 2 years of operation. Recommended : PWHT 3 hours 875 C
 