Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Incoloy 800 or Incoloy 840 which is better for immersion heater in tap water 1

Status
Not open for further replies.

alapplied

Electrical
Joined
Jun 10, 2014
Messages
2
Location
US
Incoloy 800 or Incoloy 840? Does anyone have experience which of these material is better suited (would last longer)in an application to heat tap water to create steam in small 2 to 3 gallon container?

Thanks for you help.
 
If those are your only two options then 800 is clearly superior for low temp aqueous service.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Thansk Ed,
Could you advise me why you think Incoloy 800 would be better? I did a web search looking for an anser to this quesion and did not find an adequate expaniation for why 800 is better.

Al
 
higher Cr in 800.
The Al in 840 helps form a protective oxide at high temp but does not help at all in water.
An even higher Cr alloy would be better since your heaters will never go above 300F or so.

= = = = = = = = = = = = = = = = = = = =