please give example of wps for electrods welding method of incolloy 825 pipes.
many thanks
 
Replies continue below

Recommended for you

It is unlikely that someone will provide you with an example as all contractors have their own knowhow on the subject. try contacting infill material suppliers such as SAF, lincoln or Buler Tiesen
 
Make sure part is clean and dry
No special preheat
Use overmatching consumable like 625 wire
No PWHT
 