Hello
I have some thinwall parts made of inco718. Part diameter is about 6 mm and wall thickness is about 1 mm. The problem is hardness value after heat treatment process. Heat treatment process that i did is conventional inco 718 heat treatment (solution heat treatment between 930-1010 C - min 1 hour - air cooling, 2 step aging 720 C/620 C - 8 hours/8 hours - air cooling). I changed solution temperature, cooling rates, cooling media everything that spec allows me. But i have never found a part has hardness lower than 44.5 HRc. This makes me crazy. Please help me.
Thank you.
I have some thinwall parts made of inco718. Part diameter is about 6 mm and wall thickness is about 1 mm. The problem is hardness value after heat treatment process. Heat treatment process that i did is conventional inco 718 heat treatment (solution heat treatment between 930-1010 C - min 1 hour - air cooling, 2 step aging 720 C/620 C - 8 hours/8 hours - air cooling). I changed solution temperature, cooling rates, cooling media everything that spec allows me. But i have never found a part has hardness lower than 44.5 HRc. This makes me crazy. Please help me.
Thank you.