Questions asked:
Is the pressure vessel built to ASME Boiler and Pressure Vessel Code Section VIII, Div 1 requirements? No code requirements. Company internal requirements to use pressure grade material or, if using a non pressure grade material, provide documented testing to validate the use of the material in our application.
What is the nature of the housing? Temporarily attached to pipeline like a valve during servicing. Never becomes part of permanent pipeline system. Is it welded to the pressure vessel or integral with the vessel? No, NPT threads.
What are the design service conditions? Test presure 415 psi. MaOP 285 psi. Gas, oil, water.
Of the other material that have been recommended, A148 looks good but will require testing. The others A27 , A487 require HT and / or test with each lot.
I have quotes out to other casting vendors. Thanks for the help.