Typically, Southern Pine isn't incised. Most other commonly used species are. Here is an bit from the wood handbook about incising.
"Incising is practiced primarily on Douglas-fir, western hemlock, and western larch ties and timbers for pressure treatment and on cedar and Douglas-fir poles. Incising can result in significant reductions in strength (Chap. 5)."