Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

in need of sa-516-60 allowables from 1973 code....Does anyone have this?

Status
Not open for further replies.

ThePVFabricator

Mechanical
Joined
Jan 28, 2015
Messages
5
Location
US
I need to know the allowable for that code year.
 
I have Section II Part D from 1998. This is before the Code changed from the old safety factor of 4 to the 3.5 used in the current Code. The Code was very slow moving before that and thus I would expect 1973 to have the same allowables, but perhaps someone else will have pages that old.

For SA516-60 the allowable is 15.0 ksi (60 ksi tensile divided by 4) up to 650°F. The allowable tapers off above that.
 
Contact the National Board of Boiler and Pressure Vessels. They should be able to provide copies for a fee.
 