bafometto81
Petroleum
Hi everybody,
I'm a materials engineer and I'm working as coating engineer for an oil company. I was monitoring a PQT some days ago and I saw something quite strange so I would like to ask your opinion.
The pqt was for polyurethane infill for field joint. After filling the field joint the material was errupting from the injection hole of the mould and I can not explain the behaviour of the material as I didn't expect to see that huge expansion cosifering that the material was solid not foam.
Hope you can help me,
Best regards
Nicolò Bovo
I'm a materials engineer and I'm working as coating engineer for an oil company. I was monitoring a PQT some days ago and I saw something quite strange so I would like to ask your opinion.
The pqt was for polyurethane infill for field joint. After filling the field joint the material was errupting from the injection hole of the mould and I can not explain the behaviour of the material as I didn't expect to see that huge expansion cosifering that the material was solid not foam.
Hope you can help me,
Best regards
Nicolò Bovo