Maybe someone can help me:
We measured the impulse voltage on high voltage coils. The result was, that the impulse voltage level is higher if the test is made in some steps.
E.g. one coil withstands about 50kV, if the test started with an impulse voltage of 30kV, then with 32kV, 34kV, ....
If we start with e.g. 45kV, the coil fails.
Is there any explanation for this?
We measured the impulse voltage on high voltage coils. The result was, that the impulse voltage level is higher if the test is made in some steps.
E.g. one coil withstands about 50kV, if the test started with an impulse voltage of 30kV, then with 32kV, 34kV, ....
If we start with e.g. 45kV, the coil fails.
Is there any explanation for this?