Received certifications from a foreign ductile foundry with the following mechanical and chemical properties:
106,500 psi Tensile C 2.75, Si 2.44, Mn .39, P .o1, S.02
77,700 psi Yield Cr .03, Ni .09, Mo .22, Cu .13, g .05
16% elongation
187 HRB
Material ordered was 65-45-12. Now I am no metallurgist, but these values look completely absurd and impossible. They don't even look reasonable for 100-70-03 ductile. Please let me have your thoughts.
106,500 psi Tensile C 2.75, Si 2.44, Mn .39, P .o1, S.02
77,700 psi Yield Cr .03, Ni .09, Mo .22, Cu .13, g .05
16% elongation
187 HRB
Material ordered was 65-45-12. Now I am no metallurgist, but these values look completely absurd and impossible. They don't even look reasonable for 100-70-03 ductile. Please let me have your thoughts.